Reinforcement of 2124 Al alloy with low micron SiC and nano Al2O3 via solid-state forming

Show simple item record

dc.contributor.author Gxowa, Z
dc.contributor.author Camagu, ST
dc.contributor.author Govender, S
dc.contributor.author Pereira, MF
dc.date.accessioned 2016-10-03T10:35:53Z
dc.date.available 2016-10-03T10:35:53Z
dc.date.issued 2015-07
dc.identifier.citation Gxowa, Z., Camagu, S.T., Govender, S. and Pereira, M.F. 2015. Reinforcement of 2124 Al alloy with low micron SiC and nano Al2O3 via solid-state forming. In: Seventh International Light Metals Technology Conference (LMT 2015), Port Elizabeth, South Africa, July 27-29 en_US
dc.identifier.uri http://www.scientific.net/MSF.828-829.172
dc.identifier.uri http://hdl.handle.net/10204/8775
dc.description Seventh International Light Metals Technology Conference (LMT 2015), Port Elizabeth, South Africa, July 27-29. Due to copyright restrictions, the attached PDF file only contains the abstract of the full text item. For access to the full text item, please consult the publisher's website en_US
dc.description.abstract A powder metallurgical process was used to fabricate Metal Matrix Composites (MMCs). A 2124 aluminium alloy was reinforced with 5 and 10 vol. % of Al2O3 (40-70nm) to form Metal Matrix Nano Composites (MMNCs) as well as 10 and 15 vol. % of SiC (1-10µm) to fabricate low micron MMCs. It was observed that the nano-sized Al2O3 particles were evenly dispersed in the aluminium matrix while a lot of loose SiC particles settled on the grain boundaries in the low micron MMCs. The relative density of all the composites increased due to sintering, however full densification was not achieved. This result was attributed to the hindered motion of dislocations, grains and grain boundaries by reinforcing particles. The 2124-Al/10%-SiC composite was cold extruded and the extruded part fractured. A metallographic evaluation was carried out and it was deduced that the mode of failure was intergranular cracking. Hardness tests performed after sintering indicated that hardness increased with an increase in volume fraction of reinforcement in the matrix. Annealing of the extruded part resulted in a decrease in hardness. en_US
dc.language.iso en en_US
dc.publisher Trans Tech Publication en_US
dc.relation.ispartofseries Workflow;15435
dc.subject Al/Al2O3 nanocomposite en_US
dc.subject Al/SiC composite en_US
dc.subject Powder metallurgy en_US
dc.subject Sinterability en_US
dc.subject Hardness en_US
dc.title Reinforcement of 2124 Al alloy with low micron SiC and nano Al2O3 via solid-state forming en_US
dc.type Conference Presentation en_US
dc.identifier.apacitation Gxowa, Z., Camagu, S., Govender, S., & Pereira, M. (2015). Reinforcement of 2124 Al alloy with low micron SiC and nano Al2O3 via solid-state forming. Trans Tech Publication. http://hdl.handle.net/10204/8775 en_ZA
dc.identifier.chicagocitation Gxowa, Z, ST Camagu, S Govender, and MF Pereira. "Reinforcement of 2124 Al alloy with low micron SiC and nano Al2O3 via solid-state forming." (2015): http://hdl.handle.net/10204/8775 en_ZA
dc.identifier.vancouvercitation Gxowa Z, Camagu S, Govender S, Pereira M, Reinforcement of 2124 Al alloy with low micron SiC and nano Al2O3 via solid-state forming; Trans Tech Publication; 2015. http://hdl.handle.net/10204/8775 . en_ZA
dc.identifier.ris TY - Conference Presentation AU - Gxowa, Z AU - Camagu, ST AU - Govender, S AU - Pereira, MF AB - A powder metallurgical process was used to fabricate Metal Matrix Composites (MMCs). A 2124 aluminium alloy was reinforced with 5 and 10 vol. % of Al2O3 (40-70nm) to form Metal Matrix Nano Composites (MMNCs) as well as 10 and 15 vol. % of SiC (1-10µm) to fabricate low micron MMCs. It was observed that the nano-sized Al2O3 particles were evenly dispersed in the aluminium matrix while a lot of loose SiC particles settled on the grain boundaries in the low micron MMCs. The relative density of all the composites increased due to sintering, however full densification was not achieved. This result was attributed to the hindered motion of dislocations, grains and grain boundaries by reinforcing particles. The 2124-Al/10%-SiC composite was cold extruded and the extruded part fractured. A metallographic evaluation was carried out and it was deduced that the mode of failure was intergranular cracking. Hardness tests performed after sintering indicated that hardness increased with an increase in volume fraction of reinforcement in the matrix. Annealing of the extruded part resulted in a decrease in hardness. DA - 2015-07 DB - ResearchSpace DP - CSIR KW - Al/Al2O3 nanocomposite KW - Al/SiC composite KW - Powder metallurgy KW - Sinterability KW - Hardness LK - https://researchspace.csir.co.za PY - 2015 T1 - Reinforcement of 2124 Al alloy with low micron SiC and nano Al2O3 via solid-state forming TI - Reinforcement of 2124 Al alloy with low micron SiC and nano Al2O3 via solid-state forming UR - http://hdl.handle.net/10204/8775 ER - en_ZA


Files in this item

This item appears in the following Collection(s)

Show simple item record