ResearchSpace

Scanning velocity influence on microstructure, microhardness and wear resistance performance of laser deposited Ti6Al4V/TiC composite

Show simple item record

dc.contributor.author Mahamood, RM
dc.contributor.author Akinlabi, ET
dc.contributor.author Shukla, M
dc.contributor.author Pityana, Sisa L
dc.date.accessioned 2014-01-20T10:42:28Z
dc.date.available 2014-01-20T10:42:28Z
dc.date.issued 2013-09
dc.identifier.citation Mahamood, R.M, Akinlabi, E.T, Shukla, M and Pityana, S. 2013. Scanning velocity influence on microstructure, microhardness and wear resistance performance of laser deposited Ti6Al4V/TiC composite. Materials and Design, vol. 50, pp 656-666 en_US
dc.identifier.issn 0261-3069
dc.identifier.uri http://ac.els-cdn.com/S0261306913002495/1-s2.0-S0261306913002495-main.pdf?_tid=ff0d6246-81b1-11e3-98be-00000aab0f6c&acdnat=1390208904_94495869a8899fc98e47e6beefe56561
dc.identifier.uri http://hdl.handle.net/10204/7158
dc.identifier.uri https://doi.org/10.1016/j.matdes.2013.03.049
dc.description Copyright: 2013 Elsevier. This is an ABSTRACT ONLY. The definitive version is published in Materials and Design, vol. 50, pp 656-666 en_US
dc.description.abstract Ti6Al4V is the most widely used titanium alloy in the aerospace industry because of its excellent properties. However, the wear resistance behaviour of this material is not very impressive and surface damage occurs in applications involving contact loadings. Laser material deposition process, an additive manufacturing technology offers lots of advantages in surface modification of components, repair of existing worn out parts, as well as building new components from the scratch, most especially complex components. A good control of the process parameters is inevitable to achieve the desired properties. It is easier to control a single process parameter to achieve the desired property than to control a number of the processing parameters. In this study, the influence of the scanning velocity on the evolving physical properties, the microstructure, the microhardness and the wear resistance behaviour of Ti6Al4V/TiC composite is thoroughly investigated towards achieving an effective properties control. The results showed that controlling only the scanning velocity, the physical, mechanical, metallurgical and the tribological properties of the Ti6Al4V/TiC composite can be effectively controlled. It was found that as the scanning velocity was increased, the wear resistance performance also increased, until the scanning velocity of 0.065 m/s, after which the wear resistance performance began to experience a decrease. At low scanning velocity, there were less Unmelted Carbide particles in the microstructure due to more melting of the TiC powder taking place, hence the low wear resistance performance obtained. en_US
dc.language.iso en en_US
dc.publisher Elsevier en_US
dc.relation.ispartofseries Workflow;11981
dc.subject Titanium alloys en_US
dc.subject Aerospace industry en_US
dc.subject Coefficient of friction en_US
dc.subject Laser material deposition en_US
dc.subject Microstructure en_US
dc.subject Surface roughnes en_US
dc.subject Titanium composites en_US
dc.subject Wear resistance performance en_US
dc.title Scanning velocity influence on microstructure, microhardness and wear resistance performance of laser deposited Ti6Al4V/TiC composite en_US
dc.type Article en_US
dc.identifier.apacitation Mahamood, R., Akinlabi, E., Shukla, M., & Pityana, S. L. (2013). Scanning velocity influence on microstructure, microhardness and wear resistance performance of laser deposited Ti6Al4V/TiC composite. http://hdl.handle.net/10204/7158 en_ZA
dc.identifier.chicagocitation Mahamood, RM, ET Akinlabi, M Shukla, and Sisa L Pityana "Scanning velocity influence on microstructure, microhardness and wear resistance performance of laser deposited Ti6Al4V/TiC composite." (2013) http://hdl.handle.net/10204/7158 en_ZA
dc.identifier.vancouvercitation Mahamood R, Akinlabi E, Shukla M, Pityana SL. Scanning velocity influence on microstructure, microhardness and wear resistance performance of laser deposited Ti6Al4V/TiC composite. 2013; http://hdl.handle.net/10204/7158. en_ZA
dc.identifier.ris TY - Article AU - Mahamood, RM AU - Akinlabi, ET AU - Shukla, M AU - Pityana, Sisa L AB - Ti6Al4V is the most widely used titanium alloy in the aerospace industry because of its excellent properties. However, the wear resistance behaviour of this material is not very impressive and surface damage occurs in applications involving contact loadings. Laser material deposition process, an additive manufacturing technology offers lots of advantages in surface modification of components, repair of existing worn out parts, as well as building new components from the scratch, most especially complex components. A good control of the process parameters is inevitable to achieve the desired properties. It is easier to control a single process parameter to achieve the desired property than to control a number of the processing parameters. In this study, the influence of the scanning velocity on the evolving physical properties, the microstructure, the microhardness and the wear resistance behaviour of Ti6Al4V/TiC composite is thoroughly investigated towards achieving an effective properties control. The results showed that controlling only the scanning velocity, the physical, mechanical, metallurgical and the tribological properties of the Ti6Al4V/TiC composite can be effectively controlled. It was found that as the scanning velocity was increased, the wear resistance performance also increased, until the scanning velocity of 0.065 m/s, after which the wear resistance performance began to experience a decrease. At low scanning velocity, there were less Unmelted Carbide particles in the microstructure due to more melting of the TiC powder taking place, hence the low wear resistance performance obtained. DA - 2013-09 DB - ResearchSpace DP - CSIR KW - Titanium alloys KW - Aerospace industry KW - Coefficient of friction KW - Laser material deposition KW - Microstructure KW - Surface roughnes KW - Titanium composites KW - Wear resistance performance LK - https://researchspace.csir.co.za PY - 2013 SM - 0261-3069 T1 - Scanning velocity influence on microstructure, microhardness and wear resistance performance of laser deposited Ti6Al4V/TiC composite TI - Scanning velocity influence on microstructure, microhardness and wear resistance performance of laser deposited Ti6Al4V/TiC composite UR - http://hdl.handle.net/10204/7158 ER - en_ZA


Files in this item

This item appears in the following Collection(s)

Show simple item record