Microstructure development and its influence on the properties of styrene-ethylene-butylene-styrene/polystyrene blends

Show simple item record

dc.contributor.author Banerjee, R
dc.contributor.author Ray, Suprakas S
dc.contributor.author Ghosh, AK
dc.date.accessioned 2018-12-03T12:50:05Z
dc.date.available 2018-12-03T12:50:05Z
dc.date.issued 2018-04
dc.identifier.citation Banerjee, R., Ray, S.S. and Ghosh, A.K. 2018. Microstructure development and its influence on the properties of styrene-ethylene-butylene-styrene/polystyrene blends. Polymers, vol. 10(4): 400 en_US
dc.identifier.issn 2073-4360
dc.identifier.uri https://www.mdpi.com/2073-4360/10/4/400
dc.identifier.uri https://doi.org/10.3390/polym10040400
dc.identifier.uri http://hdl.handle.net/10204/10576
dc.description This is an open access article distributed under the Creative Commons Attribution License which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited (CC BY 4.0). en_US
dc.description.abstract The present work is a novel attempt to understand the microstructure of styrene-ethylene-butylene-styrene (SEBS)/polystyrene (PS) blends not only through morphological studies, but also thermal, mechanical and rheological characterizations. SEBS/PS blends containing 10, 30 and 50 wt % PS were processed in a micro-compounder and characterized. Scanning electron microscopy (SEM) studies, with selective staining of the PS phase, revealed the presence of PS as nanometer-sized domains, as well as phase-separated micrometer-sized aggregates. Blends with 30 and 50 wt % PS exhibited a fibrillar microstructure, obeying Hirsch’s model of short fiber composites. A remarkable increase in glass transition temperature indicated a strong interaction of the fibrils with SEBS. All blends showed two modes of relaxation corresponding to the two phases. A single mode of relaxation of the PS phase has been attributed to combined effects of the partial miscibility of the added PS, along with the interaction of the fibrils with SEBS. The long relaxation time of the elastomeric phase indicated the tendency of these materials to undergo time-dependent shrinkage in secondary processing operations. An increase in PS content resulted in the lowering of the shear viscosity and energy requirement for mixing, indicating the ease of processing. en_US
dc.language.iso en en_US
dc.publisher MDPI en_US
dc.relation.ispartofseries Worklist;21729
dc.subject Polymer blends en_US
dc.subject Morphology en_US
dc.subject Fibrillar microstructure en_US
dc.subject Rheology en_US
dc.subject Mechanical properties en_US
dc.title Microstructure development and its influence on the properties of styrene-ethylene-butylene-styrene/polystyrene blends en_US
dc.type Article en_US
dc.identifier.apacitation Banerjee, R., Ray, S. S., & Ghosh, A. (2108). Microstructure development and its influence on the properties of styrene-ethylene-butylene-styrene/polystyrene blends. http://hdl.handle.net/10204/10576 en_ZA
dc.identifier.chicagocitation Banerjee, R, Suprakas S Ray, and AK Ghosh "Microstructure development and its influence on the properties of styrene-ethylene-butylene-styrene/polystyrene blends." (2108) http://hdl.handle.net/10204/10576 en_ZA
dc.identifier.vancouvercitation Banerjee R, Ray SS, Ghosh A. Microstructure development and its influence on the properties of styrene-ethylene-butylene-styrene/polystyrene blends. 2108; http://hdl.handle.net/10204/10576. en_ZA
dc.identifier.ris TY - Article AU - Banerjee, R AU - Ray, Suprakas S AU - Ghosh, AK AB - The present work is a novel attempt to understand the microstructure of styrene-ethylene-butylene-styrene (SEBS)/polystyrene (PS) blends not only through morphological studies, but also thermal, mechanical and rheological characterizations. SEBS/PS blends containing 10, 30 and 50 wt % PS were processed in a micro-compounder and characterized. Scanning electron microscopy (SEM) studies, with selective staining of the PS phase, revealed the presence of PS as nanometer-sized domains, as well as phase-separated micrometer-sized aggregates. Blends with 30 and 50 wt % PS exhibited a fibrillar microstructure, obeying Hirsch’s model of short fiber composites. A remarkable increase in glass transition temperature indicated a strong interaction of the fibrils with SEBS. All blends showed two modes of relaxation corresponding to the two phases. A single mode of relaxation of the PS phase has been attributed to combined effects of the partial miscibility of the added PS, along with the interaction of the fibrils with SEBS. The long relaxation time of the elastomeric phase indicated the tendency of these materials to undergo time-dependent shrinkage in secondary processing operations. An increase in PS content resulted in the lowering of the shear viscosity and energy requirement for mixing, indicating the ease of processing. DA - 2108-04 DB - ResearchSpace DP - CSIR KW - Polymer blends KW - Morphology KW - Fibrillar microstructure KW - Rheology KW - Mechanical properties LK - https://researchspace.csir.co.za PY - 2108 SM - 2073-4360 T1 - Microstructure development and its influence on the properties of styrene-ethylene-butylene-styrene/polystyrene blends TI - Microstructure development and its influence on the properties of styrene-ethylene-butylene-styrene/polystyrene blends UR - http://hdl.handle.net/10204/10576 ER - en_ZA


Files in this item

This item appears in the following Collection(s)

Show simple item record